Te Tikanga me te Whakamahi mo te Maka-Hanga Hangaia mo te Hiri
He aha Te Maka-Hika Hangaia Mo te Maka
Ko te rino he kirikiri kirikiri-whakakapi he mahi ki te maka i tetahi kirikiri angiangi ki runga i te kohao o roto o te miihini whakarewa (e kiia ana he pokepoke rino) hei hanga pokepokea ai. Na te mea he angiangi te paparanga kirikiri kirikiri (4 ~ 8mm), he pai ki te ohanga te whakamahi i nga taputapu whakatauira kounga-nui atu te utu. I te mutunga, kua pai ake te kounga o te maka ana, kua tino heke te para; na te kaha o te pakitara whakarewa kirikiri kirikiri kirikiri Tino pai, na reira ka tino whakapai ake i te waahanga me te taapiri o te maka.
Tiamana, te Soviet Union o mua me etahi atu whenua i tiimata ki te whakamahi i te rino kirikiri kirikiri hei whakairi i nga mahi i nga tau 1960, ko te nuinga mo te hanga i nga crankshafts rino, hubs frein, disc disc, silinder, shell bomb, tank tank me nga motuka turanga. , me etahi atu Tuhinga o mua. Ko nga rangahau tono a Haina mo te whakarewanga o te hanga rino he kirikiri kirikiri te mea i tiimata mai i nga tau moata o te 1970. I te tau 1979, i mahi ngatahi te Zhejiang Hangarau Hangarau me te Hangarau Hoahoa Yongkang me te Yongkang Tractor Factory ki te whakamahi i tenei mahi mo te wa tuatahi i roto i te hanga puranga nui o te S195 crankshaft blanks. I te wa ano, ko te arotake mahi mo te crankshaft rino haangai i hangaia e tenei mahinga i oti, i runga i te kaha o te ngoikoretanga (te whakataurite i te taumahatanga o te kaha ngenge σ-1), te pakarutanga o te whati (te whakataurite i te uara paepae thKth me te whakataurite o te whatianga K1C ) me te oranga o te ratonga (Whakataurite i te whakamatautau manawanui o te pauna 10000h), me etahi atu, he mea whakarite ki te kirikiri kirikiri kirikiri kirikiri, he pai ake i te maka kirikiri. I roto i nga tau 10 e whai ake nei, kua pai ake te whakahaere i roto i te tono. I te timatanga o nga tau 1990, e whitu nga kamupene kua whakamahi i te tikanga, ina koa ko te mahinga whakarewa kirikiri kirikiri kirikiri-kotahi mo nga poro-puoto kotahi-puoto me nga waahanga-e wha-puoto. He angitu nui. Ko nga umanga maangai i tenei waa ko te Yongkang Tractor Factory, Shangyu Power Machines Factory, Wangdu Crankshaft me te Hono Rod Factory, Wanbei Crankshaft Factory, Jinhua Internal Combustion Engine Parts Factory, Changzhou Diesel Engine Factory, me etahi atu I te 1991, i whakaaetia e te Komihana Whakamaherehere a te Kawanatanga te rino te kirikiri kirikiri kirikiri-whakakapi hei kaupapa whakatairanga hangarau hou matua mo te "Mahere E rima-Tau-Tau" o te whenua, a ka hangaia a Zhejiang Miihini me te Hiko Hoahoa Hiko hei waahanga tautoko hangarau o te kaupapa. He whakapainga nui tenei mo te hangarau whakarewa kirikiri kirikiri kirikiri a toku whenua. Ko te whakawhanaketanga te mea nui ki te whakatairanga. Whai muri i te mahinga a to maataaputanga i te kaupapa whakatairanga, i roto i nga tau e 5 ki te 6 e whai ake nei, he maha nga raru o te rino kirikiri kirikiri kirikiri mo te hanga papatipu i tino ea.
Matua:
- ①Nga hoahoa me te whakaoti i te miihini miihini whakakotahi kirikiri, i ea ai te raru roa mo te whakakii me te whakakapi i nga kaikopere matua;
- ② Ko te raina hanga-momo onepu-kirikiri whakakii i te raina whakaputa i oti me te whakariterite, a ko te taketake he hanga noa i te kirikiri-momo kirikiri-ki te hanga raina whakakai i whakapaihia ka whakamahia ki nga umanga penei i te Shanghai Nodular Iron Plant;
- ③ Ko te whakamahinga o te toenga whakarewa kirikiri kirikiri kua whakawhānuihia atu ki etahi mahi whakarakei uaua, penei i te ono-puoto crankshafts me nga crankshafts e toru-puoto;
- ④ Te whakauru i te kirikiri pani ki te hanga i te kirikiri kirikiri kirikiri, he whakapai ake i te kounga o te kirikiri kirikiri;
- ⑤ Ko te hoahoa o te mahinga whakarewa kirikiri kirikiri-whakakapi kua oti te whakarite, a kua tino pai ake te taumata hoahoa. Ko te rorohiko whaihanga rorohiko o te mahinga whakarewa kirikiri kirikiri kirikiri me te raupaparorohiko hoahoa awhinahia a te rorohiko mo te rino whakarewanga kirikiri-kua oti te hanga i te mahi whakaranga.
I tenei wa, tata ki te kotahi rau nga umanga puta noa i te motu kua tono i te huu-pania te mahi whakarira kia hua mai i te 30 nga momo castings penei i te crankshafts rino, camshafts, shafts toenga, tinana ngatata aukati-aukati, raina rango, me te aukati-kore. kōpae taputapu. Ko nga putanga o te tau e kiia ana ka maka. Tata ki te 10 × 104t. Ko nga kamupene angamaheni ko Shanghai Automobile Foundry General Ductile Iron Factory, Shenyang Nama 1 Crankshaft Factory, Guangxi Baikuang Group, Yixing Miihini General Factory, Shandong Jiuyang Group, Zhejiang Shuguang Crankshaft Factory, Benxi Tianyuan Crankshaft Factory, Baoding Film Miihini Hanga, Shanxi Lucheng Crankshaft Factory , Hebei Xinji Crankshaft Factory, me etahi atu. Heoi, he rereke nga huarahi a enei kamupene ki te whakauru i te kaupapa: kua whakawhiwhia e etahi ki ta maatau punaha ki te hoahoa, ki te hanga ranei, a ko etahi na ratou i pee me i whanake e raatau ake. Na reira, he tino rereke to raatau rangatira ki nga mahi whakarewa kirikiri kirikiri kirikiri. Ko te tango noa i te reini kirikiri kirikiri kirikiri kirikiri hei tauira, ko te maha o nga kamupene he pai ake te mohio ka taea te whakauu i te 3%, a kua tutuki nga painga ohaoha tino pai. Heoi, kei kona ano etahi kamupene he nui te tatauranga ururua o te kirikiri kirikiri kirikiri ki te 20%, he tino painga ki nga painga ohaoha o tenei mahi. Ko te take kaore i tino marama enei kamupene ki te hoahoa me nga mahi whakangao o te kaupapa, ana kaore e aro ki te whakahaere mahi.
Ko nga rongoa matua mo te hoahoatanga me te hanga tuuturu o te kirikiri kirikiri kirikiri kirikiri:
- ① Ko te matotoru o te pakitara rino me te matotoru o te kirikiri kirikiri kirikiri me te whakakotahitanga o te mea e rua ka tutuki nga whakaritenga rereke mo te whakapakaritanga me te whakamaoatanga o nga makaanga me nga matotoru o te pakitara rereke me nga taonga rereke;
- ②Whakaahua me te ohanga o te tikanga whakakikorua kirikiri kirikiri ki te whakatutuki i nga whakaritenga o nga rereketanga rereke mo te kounga o te mata me te tika o te waahanga;
- ③Tauputanga tukatuka. Pēnei i te whakatau i te punaha gating, te punaha pupuhi kirikiri, te punaha whakapau, me era atu.
- ④ Te whakatutukitanga o te mahinga papatipu. Hei tauira, te hoahoa me te hanga i te raina whakaputa me te kaihoroi pania-onepu me nga taputapu awhina;
- ⑤ Ko te whakatakoto i nga ture whakahaere, penei i nga ture o te riringi, te whakamatao me te wetewete, me te whakarereke i te waahanga whakangao.
Nga Huringa Tauhokohoko Tino O Te Maka-Utu-I Te Whakanoho I te kirikiri
Whai muri i te ringihanga o te maitai whakarewa ki roto i te whakarewa hurihuri kirikiri kirikiri kirikiri, "te kirikiri kirikiri whakakikorua-maitai" he punaha whakawhiti wera wera kore. Kia maama ai te raru, e kiia ana he iti-iti te maka. a e kiia ana ko te waahi pāmahana o ia waahanga o te punaha ka tohaina ki te raina tika. Ko te Whakaahua 1 e whakaatu ana i tetahi waahanga o te punaha. Ae ra, ko te rerenga wera motuhake ano hoki q ka whakawhiti i ia waahanga o te punaha:
E rua nga paearu whakawhiti wera e tohu ana i te kaha o te whakawhiti wera i waenga i te maka me te paparanga kirikiri kirikiri, me te miihini rino me te papa kirikiri kirikiri. k1 te ōwehenga o te ātete waiariki o te maka ki te ātete waiariki o te kirikiri onepu; Ko te k2 te ōwehenga o te ātete waiariki o te momo rino ki te ātete waiariki o te kirikiri onepu. Ki te whakaaro ki te whakakotahitanga o te k1 me te k2, me te rereketanga o te matotoru o te kirikiri kirikiri, e toru nga ahuatanga rerekee rereke e whai ake nei i waenga i te "kirikiri-kirikiri whakakikorua-rino pokepoke" tera pea ka puta:
- ① Ka k≤1 ana me k2≤1, ko te paparanga kirikiri kirikiri kei roto i te matotoru noa, ka piki ake te tere o te makariri o te makanga ka heke te matotoru o te paparanga kirikiri kirikiri.
- ②Ki te nui ake o te matotoru o te paparanga kirikiri kirikiri tetahi matotoru, kaore he painga o te peera rino ki te whakamatao o te maka. I tenei wa, he rite ki te panga onepu noa, te panga ranei i te onepu. I te mea he iti ake te kawe waiariki o te paparanga kirikiri kirikirii i te momo rino, ka maroke haere te makanga.
- HenKi te k ≧ 1 me te k2 ≧ 1, he angiangi rawa te matotoru o te kirikiri onepu, e rite ana ki te whakarewa whakarewa whakarewa.
Ko nga ahuatanga o te whakawhitinga wera i runga ake nei kua whakatutukihia e nga whakamatautau. Ka huri ana te matotoru o te paparanga kirikiri kirikiri o te crankshaft (CTЦ-14) ki te huri i te onepu-momo onepu whakarakei mai i te 4 ki te 32 mm, ka heke haere te rahi o te cimentite i roto i te anga crankshaft, me te nui o te peara me te Tuhinga o mua. Ka iti ake i te 4mm te matotoru o te paparanga kirikiri kirikiri, he rite te kaha o te makariri o te maka ki te momo whakarewa (peita matotoru); ka nui ake te paparanga kirikiri-i te 32mm, ko te kaha o te hauhautanga he rite ki te mahi onepu onepu noa.
Ka whakamahia ana te whakarewanga kirikiri kirikiri-ki te hanga i nga momo whakaari, na roto i nga whakamatau, i te tauritenga whaaho ranei hei whakatau i te matotoru o te paparanga kirikiri kirikiri me te matotoru o te rino hei whakahaere i te kaha o te maka. Hei tauira, i te hoahoanga o te 490Q rino crankshaft rino kirikiri kirikiri kirikiri kirikiri kirikiri: he matotoru o te paparanga kirikiri kirikiri he 5-8mm, a ko te matotoru o te pakitara rino he 20-30mm, e hua ana te kounga-teitei. -e haumanu haumanu kaore he parani. Ko te take nui ko:
- ① Ko te paparanga kirikiri-kirikiri te tikanga whakahaere i te reiti o te makanga, i tetahi taha, he maama noa te ahua o te maka, a, i tetahi atu ringa, he nui ake te reiti o te hauhautanga i te panga kirikiri. E whakaatu ana i te Whakaahua 2, ka ringihia ana te rino rewa ki roto i te pokepoke rino-pania o te onepu, ka heke te mahana o te makanga ki te 930 ° C i muri i te 8 meneti, ana 24 meneti kia heke iho te kirikiri onepu ki te paemahana kotahi. , a, kua piki ake te tere hauhautanga mo te 3 wa. I te mutunga, Ko nga miihini miihini whakaari ka tino whakapaihia.
- ② Kaore te kirimana rino i te tuku, engari ko te kirikiri onepu angiangi ka taea te whakaiti i te aukati o te pokepokea ai; me te kaha o te hanga auri he pai te whakamahi i te whakawhaanatanga o te whakarewa whakahekeheke i te wa o te mahinga totoka kia tutuki Kaore he ara maranga; na te kirikiri onepu angiangi, kaore i te ngawari te ahua o te kohao, a ko te tino maaka o te makanga he pai ake te whakapai ake i tera o te kirikiri kirikiri.
E rua nga paearu whakawhiti wera e tohu ana i te kaha o te whakawhiti wera i waenga i te maka me te paparanga kirikiri kirikiri, me te miihini rino me te papa kirikiri kirikiri. k1 te ōwehenga o te ātete waiariki o te maka ki te ātete waiariki o te kirikiri onepu; Ko te k2 te ōwehenga o te ātete waiariki o te momo rino ki te ātete waiariki o te kirikiri onepu. Ki te whakaaro ki te whakakotahitanga o te k1 me te k2, me te rereketanga o te matotoru o te kirikiri kirikiri, e toru nga ahuatanga rerekee rereke e whai ake nei i waenga i te "kirikiri-kirikiri whakakikorua-rino pokepoke" tera pea ka puta:
- ① Ka k≤1 ana me k2≤1, ko te paparanga kirikiri kirikiri kei roto i te matotoru noa, ka piki ake te tere o te makariri o te makanga ka heke te matotoru o te paparanga kirikiri kirikiri.
- ②Ki te nui ake o te matotoru o te paparanga kirikiri kirikiri tetahi matotoru, kaore he painga o te peera rino ki te whakamatao o te maka. I tenei wa, he rite ki te panga onepu noa, te panga ranei i te onepu. I te mea he iti ake te kawe waiariki o te paparanga kirikiri kirikirii i te momo rino, ka maroke haere te makanga.
- HenKi te k ≧ 1 me te k2 ≧ 1, he angiangi rawa te matotoru o te kirikiri onepu, e rite ana ki te whakarewa whakarewa whakarewa.
Ko nga ahuatanga o te whakawhitinga wera i runga ake nei kua whakatutukihia e nga whakamatautau. Ka huri ana te matotoru o te paparanga kirikiri kirikiri o te crankshaft (CTЦ-14) ki te huri i te onepu-momo onepu whakarakei mai i te 4 ki te 32 mm, ka heke haere te rahi o te cimentite i roto i te anga crankshaft, me te nui o te peara me te Tuhinga o mua. Ka iti ake i te 4mm te matotoru o te paparanga kirikiri kirikiri, he rite te kaha o te makariri o te maka ki te momo whakarewa (peita matotoru); ka nui ake te paparanga kirikiri-i te 32mm, ko te kaha o te hauhautanga he rite ki te mahi onepu onepu noa.
Ka whakamahia ana te whakarewanga kirikiri kirikiri-ki te hanga i nga momo whakaari, na roto i nga whakamatau, i te tauritenga whaaho ranei hei whakatau i te matotoru o te paparanga kirikiri kirikiri me te matotoru o te rino hei whakahaere i te kaha o te maka. Hei tauira, i te hoahoanga o te 490Q rino crankshaft rino kirikiri kirikiri kirikiri kirikiri kirikiri: he matotoru o te paparanga kirikiri kirikiri he 5-8mm, a ko te matotoru o te pakitara rino he 20-30mm, e hua ana te kounga-teitei. -e haumanu haumanu kaore he parani. Ko te take nui ko:
- ① Ko te paparanga kirikiri-kirikiri te tikanga whakahaere i te reiti o te makanga, i tetahi taha, he maama noa te ahua o te maka, a, i tetahi atu ringa, he nui ake te reiti o te hauhautanga i te panga kirikiri. E whakaatu ana i te Whakaahua 2, ka ringihia ana te rino rewa ki roto i te pokepoke rino-pania o te onepu, ka heke te mahana o te makanga ki te 930 ° C i muri i te 8 meneti, ana 24 meneti kia heke iho te kirikiri onepu ki te paemahana kotahi. , a, kua piki ake te tere hauhautanga mo te 3 wa. I te mutunga, Ko nga miihini miihini whakaari ka tino whakapaihia.
- ② Kaore te kirimana rino i te tuku, engari ko te kirikiri onepu angiangi ka taea te whakaiti i te aukati o te pokepokea ai; me te kaha o te hanga auri he pai te whakamahi i te whakawhaanatanga o te whakarewa whakahekeheke i te wa o te mahinga totoka kia tutuki Kaore he ara maranga; na te kirikiri onepu angiangi, kaore i te ngawari te ahua o te kohao, a ko te tino maaka o te makanga he pai ake te whakapai ake i tera o te kirikiri kirikiri.
Te Maama o te Whakamaa o Te Hinu-Uwhi-Maka
Ko nga take e awangawanga ana i te rewharewha o te hanga rino-kirikiri ki te maka i te matotoru pakitara, te maka rauemi, te whakawera i te mahana, te kirikiri kirikiri kirikiri, te kirikiri kirikiri, te matotoru o te hainoana, nga mea whakarewa rino, me te mahana i pokepokea ai. I konei, ko te awe noa o te maka o te pakitara (BC), te kirikiri o te kirikiri (bm) me te matotoru rino (bi) e korerohia ana.
Te Putanga o te bc, bm Me te bi o te Makao o te Makaa
He rereke te matotoru o te pakitara (10mm, 20mm, 40mm, 80mm, ia waa), nga kirikiri kirikiri kirikiri rereke (4mm me 32mm, ia waa) me nga momo momo rino te matotoru o te pakitara (32mm me 8mm, aua) i hangaia i raro i nga waahanga whakamatautau e whai ake nei Ko te awe o te te tere o te whakamaoatanga o te momo rino-onepu-pani: ko te hanga matū o te maka ko te 3.52% C, 2.46% Si, 0.80% Mn, 0.18% P, 0.031% S, me te kohinga matū o te kirikiri kirikiri: 90% onepu kiripaka, 8% paru, Paura puehu 2%, houku 3%
- ① Ko te matotoru o te pakitara e maka ana, ko te onepu whakakikorua kirikiri me te matotoru o te pakitara rino e pa ana ki te tere whakangawari o te maka. Na, i roto i te mahi tuuturu, me kowhiri i te matotoru pokepoke rino me te kirikiri kirikiri kirikiri kia kowhiria kia rite ki nga rereketanga o te pakitara o te peera kia whiwhi i te reiti meangiti.
- ② Ka taea te kii mai i nga matotoru rereke ma te tohu i te matotoru kirikiri kirikiri e tika ana me te matotoru o te pakitara rino kia rite te tere o te whakamatao. Hei tauira, i te Whakaahua 3, rohe ko te tikanga ko te matotoru ko te 10mm me te 20mm, ko te rohe II he 20mm me te 40mm, ko te rohe III 40mm te tikanga. Me te inaki i waenga i te awangawanga o te hihiko 80mm.
- ③ Ahakoa ka taea te whakarereke i te bm me te bi kia whiwhi i te reiti tautau mo te maka o nga matotoru rerekee, kaore e taea e nga matotoru katoa o te maka te reiti tautau. I raro i nga waahanga whakamatautau, kaore e taea te kii i nga rerenga matotoru 10mm me te matotoru 40mm Te rite o te reiti o te whakamatao (kaore he taupoki i waenga i nga kopiko).
Te kowhiringa o te kirikiri kirikiri (bm) me te matotoru o te pakitara rino (bi)
Ko te Bm me te koiora e whakatauhia ana i runga i te wheako me te whakamatautau ranei. Anei tetahi tikanga mahere, he pai mo te maka matotoru (bc) mai i te 10 ki te 80mm me te whakawera i te mahana o te 600. Ko te tikanga ko te wa meangiti. Ko te abscissa o te ānau kei te taha matau ka tohua ki te matotoru o te kirikiri kirikiri, ka taea te whakatau mai i te waa e hiahiatia ana mo te makanga e mohiotia ana kia whakamatao ki te 600 ° C me te matotoru o nga momo whakairi, me te matotoru o te pakitara e maka ana. (10, 20, 40, 80mm) e mohiotia ana, na he pai ki te whakatau i te matotoru o te kirikiri kirikiri me te matotoru o te haehae rino. Rapua te bc whaitake (hei tauira, bc = 20mm) mai i te tuaka whakapae o te haurua maui o te piko ka tuhi i tetahi raina whakapae.
Mena ka whakawhiti nga raina e rua i roto i te awhe o te kopere-a-whiti, he tohu he pai tenei maka mo te whakakakara kirikiri kirikiri. Whakawhānuitia tenei raina whakapae ki te taha matau, ka toro atu ki te rohe o bc = 20mm, ka tuhi ai i tetahi raina poutū ki raro i tenei rohe kia tae atu ki te matotoru kirikiri kirikiri e hiahiatia ana. Heoi, me kukume tenei raina poutū ki te taha matau ki te taha e taea ana kia whiwhi ai i te matotoru iti rawa o te kirikiri onepu me te matotoru o te auri rino. Mena ko te matotoru o te paparanga kirikiri kirikiri-e hiahiatia ana kia whakatauhia kaore i roto i tenei awhe, ka kitea e koe mai i te awhi o te kopere e penei ana.
- ① Ko te matotoru o te pakitara e maka ana, ko te onepu whakakikorua kirikiri me te matotoru o te pakitara rino e pa ana ki te tere whakangawari o te maka. Na, i roto i te mahi tuuturu, me kowhiri i te matotoru pokepoke rino me te kirikiri kirikiri kirikiri kia kowhiria kia rite ki nga rereketanga o te pakitara o te peera kia whiwhi i te reiti meangiti.
- ② Ka taea te kii mai i nga matotoru rereke ma te tohu i te matotoru kirikiri kirikiri e tika ana me te matotoru o te pakitara rino kia rite te tere o te whakamatao. Hei tauira, i te Whakaahua 3, rohe ko te tikanga ko te matotoru ko te 10mm me te 20mm, ko te rohe II he 20mm me te 40mm, ko te rohe III 40mm te tikanga. Me te inaki i waenga i te awangawanga o te hihiko 80mm.
- ③ Ahakoa ka taea te whakarereke i te bm me te bi kia whiwhi i te reiti tautau mo te maka o nga matotoru rerekee, kaore e taea e nga matotoru katoa o te maka te reiti tautau. I raro i nga waahanga whakamatautau, kaore e taea te kii i nga rerenga matotoru 10mm me te matotoru 40mm Te rite o te reiti o te whakamatao (kaore he taupoki i waenga i nga kopiko).
Tena koa kia mau ki te maataapuna me te wahitau o tenei tuhinga mo te taarua: Te Tikanga me te Whakamahi mo te Maka-Hanga Hangaia mo te Hiri
Minghe Kamupene Tika Raka e whakatapua ana ki te hanga me te whakarato i te kounga me te mahi nui mo te whakangao i nga waahanga (ko nga waahanga whakarewa mate whakarewa te nuinga o te waa Te Maka i te Mate Maehe-Tutuki,Te Horo Hou o te Ruma wera,Te Makarekare Whare Toi Toto), Ratonga Rauna (Ratonga Maka Mate,Miihini Cnc,Hanga Whakatika, Maimoatanga Mata). Ko nga tohu Alumini kua mate, he konupora, he Zamak / zinc / casting zinc ranei, me etahi atu whakaritenga maka e manakohia ana kia whakapiri mai ki a maatau.
I raro i te mana whakahaere o te ISO9001 me te TS 16949, ko nga mahinga katoa ka mahia i roto i nga miihini miihini whakaheke rau, miihini 5-tuaka, me etahi atu taputapu, mai i nga miihini ki nga miihini horoi horoi Ultra Sonic. roopu o nga kaiwhakangungu mohio, kaiwhakahaere me nga kaitirotiro kia pono te hoahoa a te kaihoko.
Kaihanga kirimana mo te whakaheke mate. Ko nga kaitautoko kei roto i te whare matao konumohe e mate ana i nga waahanga mai i te 0.15 lbs. ki te 6 lbs., ka whakatauhia te whakarereke tere, me te miihini. Ko nga ratonga e taapirihia ana ko te oro, te wiri, te pahekeheke, te pupuhi pupuhi, te peita, te whakakikorua, te paninga, te huihuinga, me te taputapu. Ko nga rauemi i mahi ngatahi ai ko nga kikii puri penei i te 360, 380, 383, me te 413.
Zinc mate casting hoahoa awhina / ratonga hangarau rite. Kaihanga Ritenga o te whakakautei te mate konutea. Te whakaheke i te Iti, te whakaheke i te peehi teitei, te whakaheke i te miihini maha, te miihini miihini tikanga, te mate o te waahanga me te whakaheke i te mate motuhake me te tohu o te kohao kua oti te hiri. Ka taea te hanga Castings i te roa me te whanui tae atu ki te 24 in. I roto i te +/- 0.0005 in. Manawanui.
ISO 9001: 2015 kaiwhakanao tiwhikete o te konupora maka mate, Ko nga kaha kei roto i te konupora teitei e mate ana kia tae atu ki te 200 tana ruuma wera & 3000 tana teena makariri, hoahoa taputapu, oroina, whakarewa, miihini, paura me te peita wai, QA katoa me nga kaha CMM , huihuinga, takai me te tuku.
ITAF16949 tiwhikete. Ratonga Maka Maka Taapiri Tae Atu te haumi haumi,whakarewa kirikiri,Ngakau Kari, Ngaro Kamupene ngaro,Peke Uru,He Kai Ware,Te Maka Mould Tuturu, .Mahinga he EDI, awhina hangarau, whakatauira totika me te tukatuka tuarua.
Nga Mahi Maka Maka Nga Wahanga Akoranga mo nga: Motuka, Pahikara, Papa rererangi, taonga puoro, Waiwai, taputapu Optical, Sensors, Tauira, taputapu Hiko, Whakapiringa, Karaka, Miihini, Miihini, Taonga, Taonga, Taimana, Telecom, Rama, Taputapu Hauora, taputapu Whakaahua, Karetao, Whakaahua, Taputapu Oro, Taputapu Hakinakina, Taputapu, Taonga me etahi atu.
He aha ta maatau hei awhina i a koe a muri atu?
∇ Haere ki te Wharangi Kaainga Mo Mate Maka Makaina
→Wahanga Taputapu-Rapua nga mahi i mahia e maatau.
→ Tohu Awhina mo te Mate Ratonga Maka
By Minghe Die Casting Kaihanga | Kāwai: Tuhinga Tauturu |Rauemi Tags: Tini Panuiini, Maka Maka, Makaora Maka, Te Maka Titanium, He kowiriira Casting, Maka Maka,Te Maka Koura,Whakaari Ataata,Hītori Kamupene,Porohita Mate Paratini | Korero Kore